Material Notes:
Stamford P is a standard polished grade; class "B", medium sized, leafing aluminum pigment carried in mineral spirits.Applications: Trade & Maintenance
Physical Properties Metric English Comments
Specific Gravity 1.63 g/cc
1.63 g/cc
Bulk Factor 0.074
0.074
Volatiles 27 %
27 %
Particle Size 13 µm
13 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh
1% retained
Descriptive Properties Value Comments
% Leaf (min) 55
Solvents Mineral Spirits
Water Coverage (cm²/gm) 17000