Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Silon TA 2323 HD White Catalyst Masterbatch

Category Other Engineering Material , Catalyst/Initiator
Manufacturer Silon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silon TA 2323 HD White Catalyst Masterbatch.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Masterbatch for use with SILON Silane cross-linkable PE-Xb Compounds TA 1108 HD.TA 2323 HD, together with the above mentioned graft, contains the cross-linking catalyst to complete a Sioplas System. In addition, it carries a part of the long term stabilizing system for the finished product and a special additive to protect the polymer from degradation caused by metal ions.Information provided by Silon
Physical Properties Metric English Comments
Bulk Density 0.590 g/cc
0.0213 lb/in³
Density 1.09 g/cc
0.0394 lb/in³
Volatiles <= 0.25 %
<= 0.25 %
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Users viewing this material also viewed the following: