Material Notes:
Tabond 3032 is a chemically modified LDPE / LLDPE. Its functional groups improve considerably the bonding between polar polymers, for film applications.Characteristics: • Strong adhesion to PA / PE • Adhesion durability • Polyolefin like properties and processing • Easy handling during extrusionInformation provided by Silon
Physical Properties Metric English Comments
Density 0.912 g/cc
0.0329 lb/in³
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 43.2
43.2
15s
Tensile Strength, Yield 8.10 MPa
1170 psi
Elongation at Break 343 %
343 %
Thermal Properties Metric English Comments
Melting Point 120.1 °C
248.2 °F
DSC
Descriptive Properties Value Comments
Color White