Material Notes:
Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TA 1105 HD, TA 1109 HD and TA 1117 HD. TA 2121 HD contains the cross-linking catalyst to complete together with the above-mentioned graft a Sioplas System. In addition it carries a part of the long term stabilising system for the finished product and a special additive to protect the polymer from degradation caused by metal ions.Information provided by Silon
Physical Properties Metric English Comments
Bulk Density 0.540 g/cc
0.0195 lb/in³
Density 0.960 g/cc
0.0347 lb/in³
Volatiles >= 0.050 %
>= 0.050 %
Melt Flow 8.9 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.9 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Storage Temperature <= 25.0 °C
<= 77.0 °F
Descriptive Properties Value Comments
Color White, translucent