Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Silon Taborex TA 2143 HD Catalyst Masterbatch

Category Other Engineering Material , Catalyst/Initiator
Manufacturer Silon
Trade Name Taborex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silon Taborex TA 2143 HD Catalyst Masterbatch.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Masterbatch for the use with SILON PE-Xb Compounds TA 1108 HD, TA 1132 HD and TA 1134 HD. TABOREX TA 2143 HD contains a cross-linking catalyst and a part of the long term stabilising system for the finished product. In addition it carries a special additive to protect the polymer from degradation caused by metal ions. Together with the above-mentioned grafted Polyethylene Compounds TABOREX TA 2143 HD Masterbatch forms a Sioplas System (PE-Xb) and provides processing and long term stability for the final product.Information provided by Silon
Physical Properties Metric English Comments
Bulk Density 0.540 g/cc
0.0195 lb/in³
Density 0.970 g/cc
0.0350 lb/in³
Volatiles >= 0.050 %
>= 0.050 %
Melt Flow 8.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Storage Temperature <= 25.0 °C
<= 77.0 °F
Descriptive Properties Value Comments
Color White, translucent
Users viewing this material also viewed the following: