Sinotek Materials WT85-45/75 Amorphous Graphite Powder

Category Carbon , Graphite
Manufacturer Sinotek Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sinotek Materials WT85-45/75 Amorphous Graphite Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Sinotek
Physical Properties Metric English Comments
Volatiles <= 3.4 %
<= 3.4 %
Component Elements Properties Metric English Comments
Carbon, C >= 85 %
>= 85 %
H2O <= 2.0 %
<= 2.0 %
Iron, Fe <= 0.80 %
<= 0.80 %
Descriptive Properties Value Comments
Screen Floating %, max 10