Material Notes:
Made by suspension polymerization. APPLICATIONS Extrusion : unplasticized PVC - tubes/pipes - profile - foam - sheet, film - blow moldings Calendering : unplasticized PVC - film : high temperature process Injection molding : unplasticized and plasticized PVCInformation provided by SolVin.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content <= 0.30 g/l
<= 0.30 g/l
ISO 1269
Apparent Bulk Density 0.560 g/cc
0.0202 lb/in³
ISO 60
Particle Size 63 µm
63 µm
>95% greater than value; ISO 1624
250 µm
250 µm
<5% greater than value; ISO 1624
Viscosity Test 89 cm³/g
89 cm³/g
Reduced viscosity, K value = 60; ISO 1628-2