SolVin 386NB Polyvinyl Chloride Low Viscosity Paste

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Powder
Manufacturer SolVin
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SolVin 386NB Polyvinyl Chloride Low Viscosity Paste.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Made by emulsion polymerization for plastisol preparation. MAIN APPLICATION Spread coating : - flooring top coat. ADVANTAGES - Matt appearance in flooring to coat. - Good viscosity stability on storage.Information provided by SolVin.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content <= 0.30 g/l
<= 0.30 g/l
ISO 1269
Particle Size 125 µm
125 µm
<0.15 g/kg greater than value; ISO 787-18
Viscosity Measurement 86
86
K value; ISO 1628-2