Solvay ALKAMULS® EL 620 Surfactant

Category Fluid
Manufacturer Solvay
Trade Name ALKAMULS®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ALKAMULS® EL 620 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Castor oil ethoxylate (30 EO) Emulsifier for fats, oils fatty acids and solvents. Maintains stability of oil-in-water emulsions over a wide temperature range as co-emulsifier with an HLB of around 12. Nonionic emulsifier for metal working formulations. Emulsifier for oils, fatty acids, solvents and waxes in water based formulations. Often used in textile lubricants, and in food contact formulations. Dispersant for pigments and iron powders in magnetic coupling fluids. Paper dye-leveling.Identification: CASTOR OIL ETHOXYLATE(30)CAS: 61791-12-6Available in: Asia Pacific, Europe, Latin America and North AmericaSolubility: Soluble in waterApplications: ALKAMULS EL-620 is a castor oil ethoxylate with a HLB of 12. Emulsifier for oil and waxes in water based formulations. Used as dispersant or pigments and iron powders.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.04 - 1.05 g/cc
0.0376 - 0.0379 lb/in³
pH 6.5 - 8.5
6.5 - 8.5
7% Solution
Viscosity 250 - 1000 cP
250 - 1000 cP
Optical Properties Metric English Comments
Gardner Color Number <= 4.0
<= 4.0
RP-0138
Chemical Properties Metric English Comments
Total Acid Number <= 1.0
<= 1.0
[mg KOH/g]; RP-0616
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
Karl Fisher; RP-0327
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clean, clear to slightly hazy liquid
RP-0064
HLB number 12
Odor Slight Odor
Saponification number 73-78 mg KOH/g
RP-0496