Material Notes:
Barium carbonate standard powder is used in the production of special glass, glazes, brick and tile industry, ceramic and ferrite industry. Barium carbonate standard powder is also used for removing of sulphates in phosphoric acid production and chlorine alkali electrolysis.Information provided by Solvay
Physical Properties Metric English Comments
Bulk Density 1.00 - 2.00 g/cc
0.0361 - 0.0723 lb/in³
tapped
Descriptive Properties Value Comments
Composition <0.6%
S as SO3
>99%
BaCO3/SrCO3