Physical Properties Metric English Comments
Bulk Density 1.90 - 2.00 g/cc
0.0686 - 0.0723 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 110 C Dense Refractory Castable
Description: Curon 110 C is a coarse castable. Application: covers for anode baking furnaces.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Bulk Density 1.90 - 2.00 g/cc
0.0686 - 0.0723 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 120 C Dense Refractory Castable
Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 C has good thermal shock resistance.Remarks: These values apply to cast products.Informat..
Bulk Density 1.90 - 2.00 g/cc
0.0686 - 0.0723 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 120 Dense Refractory Castable
Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 has good thermal shock resistance.Remarks: These values apply to cast products. Also avai..
Bulk Density 1.90 - 2.00 g/cc
0.0686 - 0.0723 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 120 HS Dense Refractory Castable
Description: This castable has a very good resistance against thermal shocks because of its low thermal expansion. In addition, it has a high strength. Used in incinerators and for tunnel kiln cars...
Bulk Density 1.35 - 2.00 g/cc
0.0488 - 0.0723 lb/in³
Fired
Morgan Advanced Ceramics Quartzgut Silica
Sintered, fused silica refractory materials with exceptionally low thermal conductivity and thermal expansion. Chemically inert.
Bulk Density 1.90 - 2.00 g/cc
0.0686 - 0.0723 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 130 HRC Dense Refractory Castable
Description: A coarse, low iron castable for use up to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRC has a good thermal shock resistance becaus..
Bulk Density 1.35 - 2.00 g/cc
0.0488 - 0.0723 lb/in³
Fired
Morgan Advanced Ceramics HVX Silica
Sintered, fused silica refractory materials with exceptionally low thermal conductivity and thermal expansion. Chemically inert.
Bulk Density 1.00 - 2.00 g/cc
0.0361 - 0.0723 lb/in³
tapped
Solvay Chemicals Barium carbonate standard powder
Barium carbonate standard powder is used in the production of special glass, glazes, brick and tile industry, ceramic and ferrite industry. Barium carbonate standard powder is also used for removing..