Solvay Chemicals Polyglycerol-4

Category Fluid
Manufacturer Solvay Chemicals
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals Polyglycerol-4.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyglycerol-4 is a clear yellowish viscous liquid. It is less hygroscopic than glycerol or diglycerol CAS Number: 25618-55-7Information provided by Solvay
Descriptive Properties Value Comments
Composition <1 g/kg
Water
<10%
Heptaglycerol and higher oligomers
<10%
Diglycerol
<100 mg/kg
Chloride
>75%
Sum of Di, Tri and Tetraglycerol
15-30%
Pentaglycerol and Hexaglycerol
25-45%
Tetraglycerol
30-40%
Triglycerol