Material Notes:
Information provided by Micropol Limited
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Melt Flow 1.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
9.00 MPa

@Temperature 100 °C
1310 psi

@Temperature 212 °F
ASTM D638
Elongation at Break 70 %
70 %
Modulus of Elasticity 1.50 GPa
218 ksi
0°C; ASTM D638
1.80 GPa

@Temperature 20.0 °C
261 ksi

@Temperature 68.0 °F
2.00 GPa

@Temperature -40.0 °C
290 ksi

@Temperature -40.0 °F
ASTM D638
Izod Impact, Notched 2.50 J/cm
4.68 ft-lb/in
BS 2782.306A
2.50 J/cm

@Temperature -20.0 °C
4.68 ft-lb/in

@Temperature -4.00 °F
BS 2782.306A
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature -20.0 °C
50.0 µin/in-°F

@Temperature -4.00 °F
ASTM D696
140 µm/m-°C

@Temperature 20.0 °C
77.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
500 µm/m-°C

@Temperature 100 °C
278 µin/in-°F

@Temperature 212 °F
ASTM D696
Specific Heat Capacity 2.10 J/g-°C
0.502 BTU/lb-°F
Thermal Conductivity 0.460 W/m-K
3.19 BTU-in/hr-ft²-°F
Vicat Softening Point 130 °C
266 °F
ASTM D1525