Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Chemicals Soda Solvay® Light Soda Ash (European Grade)

Category Ceramic
Manufacturer Solvay Chemicals
Trade Name Soda Solvay®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals Soda Solvay® Light Soda Ash (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass industry – Raw Material for melting; Chemical industry – Production of sodium derivatives; Detergents- Alkaline support; Metallurgical processes – Desulfurization of pig iron – Raw material for melting and Flue gas treatment – Removal of acidic components CAS Number: 497-19-8/EINECS: 207-838-8Information provided by Solvay
Physical Properties Metric English Comments
Density 0.530 - 0.570 g/cc
0.0191 - 0.0206 lb/in³
Free flowing, Typical
0.480 - 0.670 g/cc
0.0173 - 0.0242 lb/in³
Free flowing, Specification
2.533 g/cc
0.09151 lb/in³
Solubility in Water 21.4 %
21.4 %
pH 11.26
11.26
1% in water
Molecular Weight 106 g/mol
106 g/mol
Thermal Properties Metric English Comments
Melting Point 851 °C
1560 °F
Descriptive Properties Value Comments
Composition <0.04%
Na2SO4, Specification
<0.5%
NaCl, Specification
<150 ppm
CaO, Specification
<150 ppm
MgO, Specification
<30 ppm
Fe2O3, Specification
>98%
Na2CO3, Specification
0.0015
NaCl, Typical
0.01-0.02%
Na2SO4, Typical
0.573
Na2O, Specification
0.582
Na2O, Typical
0.995
Na2CO3, Typical
3-10 ppm
Fe2O3, Typical
32--60 ppm
CaO, Typical
40-78 ppm
MgO, Typical
Granulometry <25%
>0.25 mm, Typical
<5%
>1 mm, Specification
<60%
<0.063 mm, Specification
<90%
<0.125 mm, Specification
0.2-1.0%
<0.063 mm Typical
0.2-1.2%
>2 mm, Typical
0.5-2.3%
>1 mm, Typical
1.6-3%
>0.125 mm, Typical
12-40%
>0.5 mm, Typical
Loss on drying <1.5%
Specification
0.1-0.6%
Typical