Polymer Property : Density = 0.0242 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.480 - 0.670 g/cc
0.0173 - 0.0242 lb/in³
Free flowing, Specification
Solvay Chemicals Soda Solvay® Light Soda Ash (European Grade)
Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in..