Material Notes:
Description: SEQUEL® 1490 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and excellent processability. Applications: Bumper fascias and other large components that must exhibit durable paintability or excellent weatherability Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ISO 1183
Linear Mold Shrinkage 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
after bake, 80°C for 1 hr.; ISO 294
Melt Flow 34 g/10 min
34 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.5 MPa
2390 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 1.59 GPa
231 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test >= 29.4 J
>= 21.7 ft-lb
multiaxial, 2.2 m/s; ASTM D3763