Solvay GERONOL® AG 900 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name GERONOL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay GERONOL® AG 900 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Wetting agent useful in tank-mix bioactivatorsIdentification: BRANCHED NONYLPHENOL ETHOXYLATE IN ISOBUTANOLCAS: 68412-54-4, 78-83-1, 7732-18-5Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: GERONOL AG-900 is a wetting agent useful in tank-mix bioactivatorsInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 92 - 94 %

@Temperature 105 °C,
Time 7200 sec
92 - 94 %

@Temperature 221 °F,
Time 2.00 hour
RP-0541
pH 7.1 - 7.9
7.1 - 7.9
5% Solution; RP-0420
Processing Properties Metric English Comments
Moisture Content 0.40 - 0.70 %
0.40 - 0.70 %
RP-0325
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
RP-0064
Color <100
APHA, RP-0134