Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shelf Life = 6.00 Month Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Shelf Life 6.00 Month

@Temperature 4.44 °C
6.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® F-557 Phenolic Prepreg, Chopped Molding Compound Reinforced
Nelcote® F-557 is a high purity silica filler phonic resin coated on Commercial or Aerospace grade silica fabric. F-557 is used in the manufacture of intermediate temperature ablative rocket nozzle..
Shelf Life 6.00 Month

@Temperature 15.0 - 25.0 °C
6.00 Month

@Temperature 59.0 - 77.0 °F
Raschig Group 3536 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed..
Shelf Life 6.00 Month

@Temperature 15.0 - 25.0 °C
6.00 Month

@Temperature 59.0 - 77.0 °F
Raschig Group RALUPOL® 4802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u..
Shelf Life 6.00 Month

@Temperature 23.0 °C
6.00 Month

@Temperature 73.4 °F
Humiseal 1C65 Silicone Conformal Coating
Humiseal 1C65 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock ..
Shelf Life 6.00 Month

@Temperature 0.000 - 5.00 °C
6.00 Month

@Temperature 32.0 - 41.0 °F
Lord Adhesives Circalokâ„¢ EP-729 Epoxy Board Level Encapsulant
LORD Thermosetâ„¢ EP-729 encapsulant is a black, one-component epoxy specifically designed to meet the needs of coating semiconductor devices on printed circuit boards.All information provided by..
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
in original unopened containers
Master Bond MasterSil 153Med Silicone Paste for Medical Applications
Description: Master Bond MasterSil 153Med is a two component silicone compound with a paste consistency for high performance bonding and sealing. It can be used for medical device applications as it..
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
in original unopened containers
Master Bond MasterSil 708FR One Part, Flame Resistant Silicone
Description: MasterSil 708FR is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It is UL listed with a flame classification for 94V.1 for thicknesses of ..
Shelf Life 6.00 Month

@Temperature 7.22 - 12.8 °C
6.00 Month

@Temperature 45.0 - 55.0 °F
in original unopened container
Master Bond UV10TK40 UV Curable Compound Has Gap Filling Properties
Description: Master Bond UV10TK40 is a higher viscosity, one part UV system for bonding, sealing and coating with good optical clarity, excellent physical properties, chemical resistance and high gl..
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
in original unopened containers with no exposure to light
Master Bond UV25 One component, moderate viscosity UV curable system
Product Description: Master Bond UV25 is a multi-purpose, one part UV curing system for bonding, sealing, coating and encapsulation that features excellent optical clarity, good physical properties,..
Shelf Life 6.00 Month
6.00 Month
Dow Corning JCR 6115
Two-part, fast cure, low modulus LED encapsulant with low viscosity and very long working time.Information provided by Dow Corning
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Arlon 28561R015M 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. T..
Shelf Life 6.00 Month
6.00 Month
From date of manufacture
Arlon 30570R020 0.020" (0.508 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier
Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The..
Shelf Life 6.00 Month

@Temperature <=23.9 °C
6.00 Month

@Temperature <=75.0 °F
From date of manufacture
Arlon 48571R009 0.009" (0.229 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specif..
Shelf Life 6.00 Month
6.00 Month
From date of manufacture
Arlon 55579R028M 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured layer on top of a cured layer on one side This data Represents typical values for the production material. The data should not be used to write, or in place of, m..
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Arlon 55900R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: 162 Style Fiberglass Appearance: Red silicone gum on glass fabricThis data represents typical values for the p..
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Arlon R30711R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: PolyethyleneAppearance: Red silicone gum ..
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Arlon R30960T030 0.030" (0.762 mm) Uncured Silicone Rubber with Kodacel Substrate
Design/Construction:Interleave: PolyethyleneAdd-on: Uncured Silicone Rubber Substrate: Kodacel CarrierAppearance: Translucent, high viscosity gum on release linersThis data represents typical values..
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Arlon R33920W028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: White gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, ..
Shelf Life 6.00 Month

@Temperature 7.22 °C
6.00 Month

@Temperature 45.0 °F
Arlon Thermabond® 99180T010 Silicone Rubber/Fiberglass Laminate
Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Shelf Life 6.00 Month
6.00 Month
Aremco Corr-Paint™ CP4080-S1 High Temperature Protective Coating, Silicone
Shelf Life 6.00 Month
6.00 Month
Aremco Pyro-Paint™ 634-ALP High Temperature Refractory Coating
This phosphate-bonded, alumina coating system bonds exceptionally well to dense refractory ceramics, providing high abrasion and corrosion resistance for operating temperatures to 3200°F (1760°C)
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
From date of manufacture
Arlon 49100R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1681 FiberglassProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricTh..
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
Arlon 51276R015 Silicone Rubber/Fiberglass Laminate
Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
Arlon 51426W015 0.015" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the pr..
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
From date of manufacture
Arlon 55100R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricT..
Shelf Life 6.00 Month
6.00 Month
Aremco Corr-Paint™ CP4090-S High Temperature Protective Coating, Silicone-Polyester
Shelf Life 6.00 Month
6.00 Month
Aremco Pyro-Paint™ 634-YO High Temperature Refractory Coating, YO >95%
This ultra high temperature yttrium oxide coating provides exceptional protection of graphite, ceramic and metal components exposed to reactive molten metals such as titanium, uranium and their allo..
Shelf Life 6.00 Month
6.00 Month
23°C
Solvay Specialty Polymers Diofan® A 036 Polyvinylidene Chloride (PVDC)  (discontinued **)
DIOFAN® A 036 is a PVDC latex used as a flexible under layer for coating on paper and cardboard, to be covered with an appropriate topcoat.Additional Information: PROCESSING - DRYING - DIOFAN® A 0..
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Arlon 44141R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Clear PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Blue PolyethyleneThis data represent..
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Arlon 44580R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wri..
Copyright © lookpolymers.com All Rights Reserved