Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay GEROPON® AF 71 Surfactant

Category Fluid
Manufacturer Solvay
Trade Name GEROPON®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay GEROPON® AF 71 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: "GEROPON AF 71 is powdered Foam Control Agent that has been developed for construction industry. GEROPON AF 71 depresses the formation of undesired air bubbles in building products, based on hydraulic binders, during their make-up process and working. The highflowability of GEROPON AF 71 permits an easy incorporation in dry blends, or aqueous pastes with very low air content. It is universally applicable and in use both in neutral and alkaline systems, besides it shows good compatibility with other additives such as water soluble surfactants or polymers."Identification: SURFACE ACTIVE AGENT FIXED ON INERT CARRIERAvailable in: Asia Pacific, Europe, Latin America and North AmericaSolubility: Dispersible in water. Insoluble in polar adn aromatic solvents.Applications: GEROPON AF 71 is powdered Foam Control Agent that has been developed for construction industry. GEROPON AF 71 depresses the formation of undesired air bubbles in building products, based on hydraulic binders, during their make-up process and working. The high flowability of GEROPON AF 71 permits an easy incorporation in dry blends, or aqueous pastes with very low air content. It is universally applicable and in use both in neutral and alkaline systems, besides it shows good compatibility with other additives such as water soluble surfactants or polymers.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Bulk Density 0.430 g/cc
0.0155 lb/in³
pH 7.0 - 8.5
7.0 - 8.5
5% in water; RPG02
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
Descriptive Properties Value Comments
Appearance White, free flowing powder
RPG31
Composition Active content
0.5
Ionic Charge Nonionic
Users viewing this material also viewed the following: