Material Notes:
Product Description: Mackam HPC-32L is a high purity amphoteric, preservative free, surfactant that is suggested as a mild component for personal care or industrial products. Mackam HPC-32L has a higher actives/solids ratio than traditional amphoterics, which makes this product extremely cost-effective. In personal cleansing formulations such as baby shampoo or body wash, Mackam HPC-32L provides rich foam, has low irritation properties, and is non-defatting. Mackam HPC-32L is also stable over a wide pH range which makes it ideal for industrial applications such as liquid dish wash and hard surface cleaners. INCI Name: Sodium CocoamphoacetateCAS: 618104-39-5Infrared Spectrum: Matches StandardUses: Shampoos, Bubble Bath, Liquid Hand Soap, Body Wash, Liquid Dish Wash and Hard Surface CleanersInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
Solids Content 38 - 40 %
38 - 40 %
Moisture Balance
pH 8.5 - 9.5
8.5 - 9.5
Viscosity <= 500 cP
<= 500 cP
#3 SP @ 12 rpm
Optical Properties Metric English Comments
Gardner Color Number <= 3.0
<= 3.0
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
Composition Non-Carboxylate Matter
<1.8%
SMCA
<20 ppm
Sodium Chloride
6.5-8%
Total Plate Count
<20 cfu/g