Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay RHODAPEX® CO-436 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODAPEX® CO-436 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name: AMMONIUM NONYLPHENOL ETHER SULFATECAS: 68649-55-8Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODAPEX CO-436 can be used to prepare a broad range of commercial emulsion polymers including acrylics, vinyl-acrylics, and styrene-acrylics. Such polymers find application in latex paints, adhesives, paper coatings, and textiles. RHODAPEX CO-436 is particularly useful in the preparation of small particle size emulsion polymers with high water resistance and excellent chemical stability. The versatility of RHODAPEX CO-436 allows it to be used with a wide range of polymerization techniques. Including thermal and redox processes. When properly used in conjunction with other anionic and nonionic surfactants, RHODAPEX CO-436 allows fro the trouble-free commercial production of extremely stable emulsion polymers.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 58 %
58 %
60 - 64 %

@Temperature 105 °C,
Time 7200 sec
60 - 64 %

@Temperature 221 °F,
Time 2.00 hour
Oven; RP-0540
pH 6.5 - 7.5
6.5 - 7.5
10% Solution; RP-0420
Surface Tension 33 dynes/cm
33 dynes/cm
at CMC
Optical Properties Metric English Comments
Gardner Color Number <= 5.0
<= 5.0
RPG-0138
Chemical Properties Metric English Comments
Ionic Impurities - Fe (Iron) <= 5.0 ppm
<= 5.0 ppm
O-Phenanthroline; RP-0277
Processing Properties Metric English Comments
Moisture Content 20 - 25 %
20 - 25 %
Karl Fisher; RP-0327
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clean, Clear liquid
RP-0064
Composition Active
58-60%, EQ. WT. 504, RP-0026
Ethanol
12-16%, RP-0181
Critical Micelle Concentration 0.0003
Ionic Charge Anionic
Odor Alcoholic
RP-0359