Solvay RHODASURF® B7-89 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODASURF® B7-89 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: ETHOXYLATED FATTY ALCOHOLSolubility: Soluble in water and most polar solvents. Insoluble in aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Emulsifier for Agrochemical formulations. Cost-effective co-emulsifier and stabilizer for Emulsion Polymerization. Emulsifier for Personal Care formulations.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
pH 6.0 - 8.0
6.0 - 8.0
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point <= 7.50 °C
<= 45.5 °F
RPG11
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Moisture Content 10 - 12 %
10 - 12 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear liquid
RPG31
Cloud Point 58-60°C
1% in water, RPG08
Color <50 HU
Hazen, RPG23
Composition Active
0.89
Ionic Charge Nonionic