Solvay RHODOLINE® WA-120 Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODOLINE® WA-120 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Low foam APE free wetting agent.Chemical Name: PROPRIETARY SURFACTANT BLENDAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: RHODOLINE® WA-120 is a wetting agent designed for architectural paints and other coating formulations. RHODOLINE® WA-120 is APE-free, low foaming, and very easy to handle. Usage level of RHODOLINE® WA-120 is typically about 2 to 5 pounds per 100 gallons in the paint formulation.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
pH 5.5 - 7.5
5.5 - 7.5
10% Solution in water; RP-0420
Viscosity <= 500 cP
<= 500 cP
#1 sp @ 60 rpm; RP-0596
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
Karl Fisher; RP-0327
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear to Cloudy, Light Yellow Liquid
RP-0064
Cloud Point 40-45°C
1% in DW, RP-0130