Material Notes:
Description: Multipurpose dispersing agent for SC formulationsIdentification: ABSORBED SURFACTANTSolubility: Dispersible in water. Insoluble in polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North America Applications: Dispersing – Wetting agentInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Bulk Density 0.500 g/cc
0.0181 lb/in³
pH 6.0 - 8.0
6.0 - 8.0
5% in water; RPG02
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Powder
Composition Active
0.5
Ionic Charge Nonionic
Users viewing this material also viewed the following: