Solvay SUPRAGIL® MNS/90 Condensed methyl naphthalene sulfonate, sodium salt

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name SUPRAGIL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay SUPRAGIL® MNS/90 Condensed methyl naphthalene sulfonate, sodium salt.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Condensed methyl naphthalene sulfonate, sodium salt. High performance, non-foaming, dispersing agent for wide range of applications, binding properties. Specific to high conc. WG.Identification: POLYALKYL NAPHTHALENE SULPHONATECAS: 81065 – 51 – 2Solubility: Insoluble in aromatic hydrocarbons and polar solvents. Soluble in water.Available in: Asia Pacific, Europe, Latin America and North America Applications: Dispersant.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Bulk Density 0.400 g/cc
0.0145 lb/in³
pH 8.0 - 10
8.0 - 10
5% aq. Sol.; 540MA3C1E
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Moisture Content <= 8.0 %
<= 8.0 %
K. Fischer; 540MA3C09
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Fine powder brown
540MA3C1F
Composition Calcium sulfate
<1.5%, 540MA3C43
Sodium Sulfate
<10%, 540MA3C44
Ionic Charge Anionic