Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Algoflon® 25CAR B PTFE; Carbon Filled  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Conductive Carbon Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Algoflon® 25CAR B PTFE; Carbon Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer.25 wt.% Electrog. Carbon. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almost no moisture absorption, low friction coefficient, and is nonflammable.
Physical Properties Metric English Comments
Density 2.12 g/cc
0.0766 lb/in³
ASTM D792
Apparent Bulk Density 0.450 g/cc
0.0163 lb/in³
ASTM D4894
Linear Mold Shrinkage 0.024 cm/cm
0.024 in/in
Radial shrinkage of 10 cm o.d. sintered rod at 23°C
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
Tensile Strength, Ultimate 21.0 MPa
3050 psi
ASTM D638
Elongation at Break 220 %
220 %
ASTM D638
Coefficient of Friction, Dynamic 0.060
0.060
ASTM D1894
Coefficient of Friction, Static 0.080
0.080
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 140 µm/m-°C

@Temperature 23.0 - 250 °C
77.8 µin/in-°F

@Temperature 73.4 - 482 °F
ASTM D696
Thermal Conductivity 0.600 W/m-K
4.16 BTU-in/hr-ft²-°F
ASTM C177
Maximum Service Temperature, Air 260 °C
500 °F
Continuous Service