Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Diofan® A 602 Polyvinylidene Chloride (PVDC)

Category Polymer , Thermoplastic , PVDC , Polyvinyl Dichloride (PVDC)
Manufacturer Solvay Specialty Polymers
Trade Name Diofan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Diofan® A 602 Polyvinylidene Chloride (PVDC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Diofan® A 602 is a water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances.It features strong barrier properties to water vapor and very low water absorption. Diofan® A 602 also offers very good resistance to oil and benzene. Due to a very low MFFT, this waterborne binder can be applied at low temperature as a flexible and tack free film.Features: Flame Retardant; Low to No Water Absorption; Moisture Barrier; Non-Toxic; Oil Resistant; Oxygen BarrierUses: Barrier Coatings; Coating ApplicationsAdditional Properties: Density - 1.580 g/cm³; Density - 1.260 g/cm³; Emulsion Type - Anionic; Filmability - 5 °C; Oxygen Transmission Rate - ASTM D3985 > 1000 cm³/m²/bar/24 hr; pH - 4.0; Shelf Life - 12 month; Solids Content - 55 %; Surface Tension - 33 mN/m; Viscosity - (23°C): 19 mPa·sInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Water Vapor Transmission 160 g/m²/day

@Thickness 0.00100 mm,
Temperature 38.0 °C
10.3 g/100 in²/day

@Thickness 0.0000394 in,
Temperature 100 °F
90% RH; ASTM F1249
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 7.00 °C
44.6 °F
DSC
Descriptive Properties Value Comments
Agency Ratings EC 1907/2006 (REACH); EU No 10/2011
Availability Asia Pacific
Europe
Latin America
North America
Color Milky White
Form Liquid
Users viewing this material also viewed the following: