Solvay Specialty Polymers FOMBLIN® LC55 PFPE Lubricant

Category Fluid , Lubricant , Perfluoropolyether (PFPE)
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name FOMBLIN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers FOMBLIN® LC55 PFPE Lubricant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requiring low viscosity.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.87 g/cc
0.0676 lb/in³
ASTM D891
Viscosity Measurement 92
92
Viscosity Index; ASTM D2270
Kinematic Viscosity 53 cSt

@Temperature 20.0 °C
53 cSt

@Temperature 68.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 21.5 cSt
21.5 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 4.2 cSt
4.2 cSt
ASTM D445
Molecular Weight 1700 g/mol
1700 g/mol
Evaporation Loss 2.5 %
2.5 %
22 hrs. at 60°C; ASTM 2595
40 %
40 %
22 hrs. at 120°C; ASTM 2595
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 100 kg
221 lb (mass)
Mean Hertz Load; IP 239
400 kg
882 lb (mass)
Welding Load; IP 239
Four Ball Wear 0.600 mm
0.0236 in
Avg. scar diameter; ASTM D4172
Thermal Properties Metric English Comments
Pour Point -56.0 °C
-68.8 °F
ASTM D97
Descriptive Properties Value Comments
Approximate ISO Grade 22
Oxygen Impact (BAM) 100°C, Impact Pressure 160 atm