Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Four Ball Extreme Pressure, Weld Load = 400 kg Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
Welding Load; IP 239
Solvay Specialty Polymers FOMBLIN® LC200 PFPE Lubricant
FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
Welding Load; IP 239
Solvay Specialty Polymers FOMBLIN® LC55 PFPE Lubricant
FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
Welding Load; IP 239
Solvay Specialty Polymers FOMBLIN® LC80 PFPE Lubricant
FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
ConocoPhillips Tacna® EP Polyurea Grease NLGI Grade 1
Description: Conoco Tacna EP Polyurea Grease is a shear-stable product with exceptional extreme-pressure characteristics and excellent water resistance. It is recommended for use in steel mills, off..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
ConocoPhillips Tacna® Rx NLGI No. 1
Description: Conoco Tacna Rx is a multipurpose, lithium-complex, polymer-enhanced grease designed for a wide range of applications, including passenger cars, agricultural equipment, race cars, motor..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
Dow Corning MOLYKOTE® 3451 CHEMICAL RESISTANT BEARING GREASE
Fluorosilicone grease thickened with PTFEInformation provided by Dow Corning
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
Dow Corning MOLYKOTE® 3452 CHEMICAL RESISTANT VALVE GREASE
Fluorosilicone grease thickened with PTFEInformation provided by Dow Corning
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
Dow Corning MOLYKOTE® G-0103 GREASE
Mineral base multi-service grease designed for extended lubrication of bearingsInformation provided by Dow Corning
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
ASTM D2596, DIN 51 350
Chesterton 787 Sliding Paste
Description: Chesterton® 787 Sliding Paste is a premium quality pure synthetic lubricant that will function affectivity even at ultra high temperatures and pressures. Designed for the most severe o..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
ASTM D2596, DIN 51 350
Chesterton 785 Parting Lubricant
Description: Chesterton® 785 Parting Lubricant represents the newest generation of anti-seize compound. A proprietary blend of ultra-fine inorganic solid lubricants in a non-carbonizing, ashless sy..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
Weld Point
ChevronTexaco Delo® NLGI 0 Grease EP
FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
Weld Point
ChevronTexaco Delo® NLGI 00 Grease EP
FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
ConocoPhillips 1 Milube® Grease 2100 NLGI No. 1
Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic ..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
1770 rpm, 80°F (27°C); ASTM D-2596
ConocoPhillips EP Polyurea NLGI Grade No. 1
Polyurea Greases offer significant performance advantages in high temperature, multipurpose, long-life and wet applications over conventional soap thickened greases. The nonsoap, polyurea thickener,..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
ASTM D 2596
ConocoPhillips Gear Shield NC Open Gear Lubricant
Description: Conoco Gear Shield NC is a black, viscous fluid designed to lubricate open gears. Gear Shield NC contains neither chlorinated solvents nor lead compounds. Gear Shield NC is designed to ..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
Weld Point
ChevronTexaco Black Pearl® NLGI 1 Grease EP
FeaturesChevron Black Pearl Greases EP are multipurpose, extreme pressure, water-resistant greases.They are formulated with ISOSYN® base stock, a polyurea thickener, and rust and oxidation inhibito..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
Weld Point
ChevronTexaco Black Pearl® NLGI 2 Grease EP
FeaturesChevron Black Pearl Greases EP are multipurpose, extreme pressure, water-resistant greases.They are formulated with ISOSYN® base stock, a polyurea thickener, and rust and oxidation inhibito..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
ChevronTexaco Coupling Grease NLGI Grade 0/1
Texaco Coupling Grease delivers value through:Superior film strength — Formulated with a high viscosity base oil and polymer for superior film strengthLittle to no oil separation in high-speed coup..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
ConocoPhillips 1 Milube® Grease 2100T NLGI No. 1
Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic ..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
ASTM D-2596
ConocoPhillips 595 NC Open Gear Lube
Description: Conoco Open Gear Lube 595 NC is a black, viscous, semi-fluid product that can be applied via central pumping systems that utilize injectors and nozzles for spray or drip application. Op..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
1770 rpm, 80°F (27°C); ASTM D-2596
ConocoPhillips EP Polyurea NLGI Grade No. 2
Polyurea Greases offer significant performance advantages in high temperature, multipurpose, long-life and wet applications over conventional soap thickened greases. The nonsoap, polyurea thickener,..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
ASTM D2596
ConocoPhillips Grade 1 Calcium M Grease NLGI
Description: Conoco Calcium M Grease is a specialty product that incorporates high load-carrying and antiwear capabilities with excellent low temperature properties and high-temperature stability af..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
ConocoPhillips Tacna® Rx NLGI No. 2
Description: Conoco Tacna Rx is a multipurpose, lithium-complex, polymer-enhanced grease designed for a wide range of applications, including passenger cars, agricultural equipment, race cars, motor..
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
Weld Point
ChevronTexaco Ulti-Plex® NLGI 1 Greases EP
FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.The..
Copyright © lookpolymers.com All Rights Reserved