Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Halar® 3404DA Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)

Category Polymer , Thermoplastic , Fluoropolymer , ETFE/ECTFE , ECTFE Fluoropolymer
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Halar® 3404DA Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Halar® 3404DA is a filled, pearl-white, semicrystalline melt processable fluorinated resin that may be used in full compliance with the federal Food, Drug and Cosmetic Act food additive regulation 21 CFR 177.1380(a)(4). It is designed for electrostatic powder coatings and in protection and anti-corrosion applications where food contact compliance is required. Halar® 3404DA provides superior water vapour permeation resistance compared to Halar® 6014. It also exhibits very good chemical, electrical and thermal properties. Additionally Halar® 3404DA coatings show very good surface finish and hardness. Main features of Halar® 3404DA include: - Food contact compliance - Very good chemical resistance - Very good thermal properties - Optimum permeation resistance - Outstanding flame resistance - Very good surface characteristics - PurityAdditional Information: Processing - Halar® 3404DA can be processed using normal electrostatic powder coating techniques. Generally the procedure involves substrate preparation, spray coating, baking and cooling. Depending on the application further processing can be carried out. Several passes maybe required to obtain the desired Halar load and build up coating thickness. - Halar® 3404DA can be used neat and without any further formulation. Substrate preparation, gun parameters such as voltage and both oven temperature and time must all be well controlled to achieve defect free coated items. Storage and Handling - Halar® melt processable fluoropolymer resins can be stored without shelf life issues when kept in a clean and dry area at ambient temperatures. Opened containers should be tightly resealed to prevent any contamination. Safety and Toxicology - Before using Halar® melt processable fluoropolymer resins consult the product Material Safety Data Sheet and follow all label directions an handling precautions. - As with all fluoropolymer materials, handling and processing should only be carried out in well ventilated areas. Vapor extractor units should be installed above processing equipment. Fumes must not be inhaled and eye and skin contact ought to be avoided. In case of skin contact wash with soap and water. In case of eye contact flush with water immediately and seek medical help. Do not smoke in areas contaminated with powder, vapor or fumes. - See Material Safety Data Sheet for detailed advice on waste disposal methods. Packaging - Halar® 3404DA is packaged in 25kg non returnable drums. Each drum has two bags liner made of polyethylene resin.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ASTM D3275
Particle Size 28 µm
28 µm
Method C; Internal Method
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 275 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ASTM D3275
Thermal Properties Metric English Comments
Melting Point 242 °C
468 °F
ASTM D3275
Descriptive Properties Value Comments
Agency Ratings FDA 21 CFR 177.1380(a)(4)
Appearance White
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Food Contact Acceptable
Good Chemical Resistance
Good Corrosion Resistance
Good Electrical Properties
Good Surface Finish
Good Thermal Stability
High Hardness
High Purity
Semi Crystalline
Filler Unspecified FillerReinfor.
Forms Powder
Generic ECTFE
Processing Method Coating
Uses Coating Applications
Users viewing this material also viewed the following: