Solvay Specialty Polymers Halar® 9414 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE), Filled

Category Polymer , Thermoplastic , Fluoropolymer , ETFE/ECTFE , ECTFE Fluoropolymer
Manufacturer Solvay Specialty Polymers
Trade Name Halar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Halar® 9414 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE), Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Halar® 9414 is a filled, pearl-white, semicrystalline melt processable fluorinated resin. It is designed for electrostatic powder coatings and can be used as a primer, intermediate or topcoat in protection and anti-corrosion applications.Features: Good Chemical Resistance; Good Corrosion Resistance; Good Electrical Properties; Good Surface Finish; Good Thermal Stability; High Hardness; Semi CrystallineUses: Coating ApplicationsAdditional Properties: Average Particle Size - Internal Method 28 µmInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ASTM D1505
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 275 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 242 °C
468 °F
DSC
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color White
Form Powder
Processing Technique Coating