Solvay Specialty Polymers Hylar® Latex 932 Polyvinylidene Fluoride (PVDF)

Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer Solvay Specialty Polymers
Trade Name Hylar®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Hylar® Latex 932 Polyvinylidene Fluoride (PVDF).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hylar® Latex 932 is a stabilized aqueous dispersion that contains approximately 22% by weight of a high molecular weight PVDF polymer (polyvinylidene fluoride) of medium crystallinity. The dispersion contains a non-ionic surfactant to stabilize against coagulation by conventional means. Hylar® Latex 932 is useful for applications such as water-based coatings and fabric impregnation.Features: Clean/High Purity; Crystalline; Good Strength; Good Toughness; Good UV Resistance; Good Weather Resistance; High Gloss; High Molecular Weight; Low to No Odor; Radiation (Gamma) ResistantUses: Coating Applications; FilmAdditional Properties: Brookfield Viscosity - 2 to 6 mPa·s; Particle Size - 0.200 to 0.400 µm; pH - 3.0 to 4.0; Solids Content - 20.0 to 25.0 wt%Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Viscosity 2.90e+6 - 3.30e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
2.90e+6 - 3.30e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Thermal Properties Metric English Comments
Melting Point 156 - 160 °C
313 - 320 °F
DSC
Descriptive Properties Value Comments
Availability Europe; North America
Color White
Form Latex