Ineos G36-24-150 is a medium density polyethylene resin designed for geomembrane sheet extrusion. The resin has excellent environmental stress crack resistance (ESCR).Natural resin; some physical properties may be specific to the carbon black filled resin.
Physical Properties Metric English Comments
Density 0.937 g/cc
0.0339 lb/in³
ASTM D4883
Environmental Stress Crack Resistance >= 3000 hour
>= 3000 hour
Condition B and C; ASTM D1693
Oxidative Induction Time (OIT) >= 100 min
>= 100 min
at 200°C, black product - aluminum pan method
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
High Load Melt Index 22 g/10 min
22 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ASTM D2240
Tensile Strength, Ultimate 27.5 MPa
3990 psi
2 in/min.; ASTM D638
Tensile Strength, Yield 17.5 MPa
2540 psi
2 in/min (50 mm/min); ASTM D638
Elongation at Break >= 800 %
>= 800 %
2 in/min (50 mm/min); ASTM D638
Flexural Modulus 0.575 GPa
83.4 ksi
Tangent-Method 1; ASTM D790
Izod Impact, Notched 4.00 J/cm
7.49 ft-lb/in
Partial break
Thermal Properties Metric English Comments
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Descriptive Properties Value Comments
Process Sheet Extrusion