Solvay Specialty Polymers Polidiemme® G/420 Thermoset Elastomer (TSE)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Solvay Specialty Polymers
Trade Name Polidiemme®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Polidiemme® G/420 Thermoset Elastomer (TSE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (Sioplas® method)Standards complying: Cenelec HD 22.1 EI7; Cenelec HD 603 DIH1, DIH2 and DIH3; IEC 60502 EPR and HEPR; IEC 60092/351 EPR and HEPR; BS 7655 GP4, GP5, GP6 and GP7; EN 50363-0 G7; VDE 0207/20 3GI3Features: Crosslinkable; Low ToxicityUses: Low Voltage Insulation; Power Cable Jacketing; Wire & Cable ApplicationsAdditional Properties: Change in Bend Test - IEC 60811 (150°C): No cracks; Collar Temperature - 170 to 190 °C; Head Temperature - 170 to 190 °C; Hot Set - IEC 60811 30 %; Hot Set - IEC 60811 0.0 %; Hot Set - IEC 60811 50 %; Hot Set - IEC 60811 0.0 %; Insulation Resistance Constant - IEC 60502 (20°C): 15000 Mohm·km; Insulation Resistance Constant - IEC 60502 (90°C): 5000 Mohm·km; Water Absorption - IEC 60811 (100°C): 1.00 mg/cm²Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792
Melt Flow 1.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 32
32
ISO 868
Tensile Strength at Break 20.5 MPa
2970 psi
ASTM D638
Elongation at Break 470 %
470 %
ASTM D638
Tensile Modulus 0.00700 GPa
1.02 ksi
ISO 527-2
Electrical Properties Metric English Comments
Volume Resistivity 1.30e+15 ohm-cm

@Temperature 90.0 °C
1.30e+15 ohm-cm

@Temperature 194 °F
ASTM D257
4.10e+15 ohm-cm

@Temperature 20.0 °C
4.10e+15 ohm-cm

@Temperature 68.0 °F
ASTM D257
Dielectric Constant 2.3

@Frequency 1000 Hz
2.3

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 39.0 kV/mm
991 kV/in
ASTM D149
Dissipation Factor 0.00080

@Frequency 1000 Hz
0.00080

@Frequency 1000 Hz
ASTM D150
Processing Properties Metric English Comments
Zone 1 140 - 160 °C
284 - 320 °F
Zone 2 150 - 170 °C
302 - 338 °F
Zone 3 160 - 180 °C
320 - 356 °F
Zone 4 170 - 190 °C
338 - 374 °F
Die Cooling Temperature 180 - 220 °C
356 - 428 °F
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following: