Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 39.0 kV/mm | 991 kV/in | ASTM D149 |
PolyOne Syncure™ System S110FV Polyethylene, Crosslinked (XLPE) Syncure™ systems are two part moisture crosslinkable compounds, is a UL bulletinized high strength, highly flame retardant insulation compound. Available in a RoHS complaint version.NOTE: The above.. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | ASTM D149 |
PolyOne Syncure™ System S112BL Polyethylene, Crosslinked (XLPE) Syncure™ systems are two part moisture crosslinkable compounds. S112BL is a CSA listed, high strength, weather resistant, black (2.5% carbon black) cable insulation compound. RoHS compliant.STORAGE.. |
|||
Dielectric Strength | 39.0 - 49.0 kV/mm | 991 - 1240 kV/in | Average value: 44.7 kV/mm Grade Count:3 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Dielectric Strength | 39.0 - 122 kV/mm | 991 - 3100 kV/in | Average value: 78.8 kV/mm Grade Count:6 |
Overview of materials for Solventless Epoxy Varnish, Electrical Insulation This property data is a summary of similar materials in the MatWeb database for the category "Solventless Epoxy Varnish, Electrical Insulation". Each property range of values reported is minimum and.. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | ASTM D149 |
Solvay Specialty Polymers Polidiemme® G/420 Thermoset Elastomer (TSE) Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (Si.. |
|||
Dielectric Strength | 39.0 kV/mm @Thickness 1.57 mm |
991 kV/in @Thickness 0.0618 in |
ASTM D149 |
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP), 30% Glass Fiber Xydar® G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology.The moldab.. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | K20/P50; IEC 60243-1 |
Styrolution Luran® 378 P G7 35% Glass Filled SAN Description: Glass-reinforced grade with very high stiffness and low thermal coefficient of liner expansion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Dielectric Strength | 39.0 kV/mm @Thickness 1.50 mm |
991 kV/in @Thickness 0.0591 in |
Short Time; IEC 60243-1 |
Styrolution Novodur® HH-106 ABS Novodur HH-106 is a high heat injection molding grade providing a balanced property profile.Information provided by Styrolution |
|||
Dielectric Strength | 39.0 kV/mm @Thickness 1.00 mm |
991 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Styrolution Novodur® P2M-V ABS Pellets Novodur® P2M-V has high impact strength, high gloss, and low emission. It is used for the production of molded plastic articles. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | K20/P50; IEC 60243-1 |
Styrolution Terluran® HH-106 Q109 Colored ABS Description: Injection-molding grade with high resistance to heat deformation and impact, with improved surface quality suitable for automotive applications.Information provided by STYROLUTION, whic.. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | |
Von Roll Isola IMI Varnish 74010A Epoxy Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: 19°C. Average solids: 60%. Usage Notes: Use with IMI 74010 hardener for final coat over field coils, windings, and heavy duty motors. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | ASTM D149 |
Unitika U-100 Engineering Plastic CAS No: 26590-50-1Information provided by Unitika Ltd. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® 1SBVX-50H LDS black PA1010-GF50 Product Description: Grilamid 1SBVX-50H LDS black is a 50% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno.. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® AG-30 H PA66 Product description: Grilon AG-30 H black 9836 is a normal viscosity, specially heat stabilized PA 66 injection molding grade with 30% glass fibres. Grilon AG-30 H black 9836 has the following impor.. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® BFZ 3 PA6 Product description: Grilon BFZ 3 is an unreinforced, high impact resistant PA6 extrusion grade. Grilon BFZ 3 has the following important properties: Extreme toughnessEasy processingLow density Gril.. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 410 Paper, 2 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 410 Paper, 3 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 3982 PA12 Product description: Grilamid XE 3982 is a highly flexible extrusion grade, based on Polyamide 12 with following main attributes: High flexibilityLow plasticizer migration (low blooming)Very good ch.. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4181 black PA1010 Product description: Grilamid XE 4181 black 9992 is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4181 black 9992 is highly .. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4181 nat PA1010 Product description: Grilamid XE 4181 natural is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4181 natural is highly resist.. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | 50%RH; IEC 60243-1 |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST801 is an unreinforced super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity r.. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | |
Arkema Group Pebax® 4033 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | DIN 53481/VDE 0303 |
BASF Elastollan® 1180A Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | IEC 243/1 |
BASF Ultradur® B 6550 LN PBT Description: High-viscosity grades for the extrusion of loose buffer tubes for optical fibers, semi-finished products for machining, profiles and pipes.Information provided by BASF |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | ASTM D149 |
PolyOne Syncure™ System S100FH Polyethylene, Crosslinked (XLPE) Syncure™ systems are two part moisture crosslinkable compounds. S100FH is a UL bulletinized, flame retardant cable insulation compound. Available in a RoHS compliant version.NOTE: The above represe.. |
|||
Dielectric Strength | 39.0 kV/mm @Thickness 1.57 mm |
991 kV/in @Thickness 0.0618 in |
ASTM D149 |
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP)
(Unverified Data**) Xydar G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology. The moldabili.. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | ASTM D149 |
PolyOne Syncure™ System S100NA Polyethylene, Crosslinked (XLPE) Syncure™ systems are two part moisture crosslinkable compounds, UL bulletinized easy processing, high strength, colorable cable insulation compound suitable for service entrance cables. RoHS compli.. |
|||
Dielectric Strength | 39.0 kV/mm | 991 kV/in | ASTM D149 |
PolyOne Syncure™ System S110FV-UV Polyethylene, Crosslinked (XLPE) Syncure™ systems are two part moisture crosslinkable insulation compounds. S110FV-UV is a UL bulletinized, RoHS compliant, high strength, highly flame retardant insulation compound. Available in bl.. |