Solvay Specialty Polymers solvene® 250 EAP Electroactive Polymer (EAP)

Category Polymer , Thermoplastic
Manufacturer Solvay Specialty Polymers
Trade Name solvene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers solvene® 250 EAP Electroactive Polymer (EAP).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Annealing Temperature - < 135 °C; Breakdown Voltage - 250 kV/mm; Coercive Field - 50 kV/mm; Crystallization Point - ASTM D3418 123 °C; Curie Temperature - ASTM D3418 110 °C; d33 - -38.0 pC/N; Kt - 35 %; Molecular Weight - ISO 16014-1 75 to 500; Poling Field - < 200 kV/mm; Remanent Polarization - < 10.0 µc/cm²Information provided by Solvay Specialty Polymers.
Mechanical Properties Metric English Comments
Tensile Strength at Break 49.0 - 54.0 MPa
7110 - 7830 psi
ASTM D638
Tensile Strength, Yield 22.0 - 28.0 MPa
3190 - 4060 psi
ASTM D638
Elongation at Break 400 - 600 %
400 - 600 %
ASTM D638
Elongation at Yield 9.0 - 12 %
9.0 - 12 %
ASTM D638
Tensile Modulus 0.550 - 0.850 GPa
79.8 - 123 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 144 °C
291 °F
ASTM D3418
Electrical Properties Metric English Comments
Dielectric Constant 15

@Frequency 1.00e+6 Hz
15

@Frequency 1.00e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
Form Powder