Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15 V25 is recommended in all industrial parts, offering a good combination between thermal and mechanical properties. This grade is commonly used in the automotive industry to mould large parts with a low warpage, such as: rocker cover, car body parts, engine covers. This product is available in black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
ISO 527 Type 1A
Elongation at Break 5.0 %
5.0 %
ISO 527 Type 1A
Tensile Modulus 5.50 GPa
798 ksi
ISO 527 Type 1A
Flexural Modulus 5.00 GPa
725 ksi
ISO 178
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+14 ohm-cm
3.00e+14 ohm-cm
IEC 60093
Surface Resistance 3.00e+11 ohm
3.00e+11 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC 60250
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 60243
Dissipation Factor 0.080
0.080
IEC 60250
Comparative Tracking Index 425 V
425 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %