Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | |
Polimeri Europa EDISTIR PD RK4514H High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,093-06-07-23 UL94 V-2, polybromodiphenylether (PBBE) free, antimony free, HIPS satisfying at 960°C the glow wire test.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179/1eU |
Pasargad Polymer Peyvand Pasamid 3P-H1130B Nylon 6, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179/1eU |
Pasargad Polymer Peyvand Pasamid 3P-H7130B Nylon 6/66, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Charpy Impact Unnotched | 8.00 - 10.5 J/cm² | 38.1 - 50.0 ft-lb/in² | Average value: 9.33 J/cm² Grade Count:6 |
Overview of materials for Nylon 63, 35% Glass-Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 50/TF/15/GY04 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® H605 Low emission, easy flowing.,Property data per ISO test methods. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179/1eU |
Lucite International Diakon® ST50G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | |
LATI Latamid SP1 G/50 PA 6.10, 50% Glass Fiber Reinforced Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYLSTARâ„¢ S 218 V35 PA6, 35% glass filled, Conditioned Description: TECHNYL STAR Polyamide, reinforced with 35% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Europe and North America .. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO Data, Low Temp |
Styron Magnum™ 2620 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, Conditioned Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179-1 |
Unitika B2040G33 PA66, 33% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BG-40 FC PA6-GF40 Product description: Grilon BG-40 FC is a heat stabilized PA6 injection molding grade with 40% glass fibers. Grilon BG-40 FC has the following important properties: High stiffnessExcellent surface f.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Stanyl® TW241F12 (DAM) Nylon 46 60% Glass Reinforced, Heat Stabilized, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GV-5H EF nat PA*-GF50 Product description: Grivory GV-5H EF natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GV-5H PA*-GF50 Product description: Grivory GV-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® GV-6 FWA nat PA*-GF60 Product description: Grivory GV-6 FWA natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GV-6 FWA nat PA*-GF60 Product description: Grivory GV-6 FWA natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-50/4 FA PA666-GF50 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® TSG-50/4 PA666-GF50 Product description: Grilon TSG-50/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50/4 has the following important properties: High sti.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4065 black 9238 PA*-GF50 Product description: Grivory XE 4065 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4108 black 9992 PA612-GF50 Product description: Grilamid XE 4108 black 9992 is a 50% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4108 are: low water absorpti.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GV-6H black PA*-GF60 Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® GVL-4H black 9915 PA*-GF40 Product description: Grivory GV-6H EF natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GVS-5H black 9915 PA*-GF50 Product description: Grivory GVS-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® HT1V-5 FWA nat PA6T/6I-GF50 Product description: Grivory HT1V-5 FWA natural is a 50 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry) Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | |
Biomer P240 PHB Biodegradable Polymer PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179 |
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Conditioned) Ultramid 1703-2 BK ND3007 is a 25% glass reinforced, heat stabilized injection molding nylon 6/6. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GV-5 FWA nat PA*-GF50 Product description: Grivory GV-5 FWA natural is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |