Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Available in: Europe and North AmericaProduct Applications: TECHNYL® A 218G1 V25 BLACK 34N is particularly recommended for the injection molding of parts in permanent contact with cooling liquids in cars, such as: - cooling and heating radiator systems, header tanks, thermostat components, inlet / outlet pipes. This product is available in black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Elongation at Break 4.0 %
4.0 %
ISO 527 Type 1A
Tensile Modulus 6.30 GPa
914 ksi
ISO 527 Type 1A
Flexural Strength 155 MPa
22500 psi
ISO 178
Flexural Modulus 5.00 GPa
725 ksi
ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 2.70 J/cm²
12.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 29.0 kV/mm
737 kV/in
IEC 60243
Dissipation Factor 0.11
0.11
IEC 60250
Comparative Tracking Index 425 V
425 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %