Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech SP-9030 Economy ABS Sheet

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Sheet
Manufacturer Spartech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech SP-9030 Economy ABS Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: ABS SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Tensile Modulus 2.00 GPa
290 ksi
ASTM D638
Flexural Yield Strength 55.2 MPa
8000 psi
ASTM D790
Flexural Modulus 2.14 GPa
310 ksi
ASTM D790
Izod Impact, Unnotched 2.67 J/cm
5.00 ft-lb/in
ASTM D256
0.747 J/cm

@Temperature -40.0 °C
1.40 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Falling Dart Impact 20.3 J
15.0 ft-lb
73°F; ASTM D3029
8.13 J

@Temperature -40.0 °C
6.00 ft-lb

@Temperature -40.0 °F
ASTM D3029
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
190 °F
ASTM D648
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Gloss 90 %
90 %
Gardner; ASTM D2523
Users viewing this material also viewed the following: