Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Plaskolite Vivak PETG Sheet VIVAK offers a balance of physical properties and ease of fabrication. It is ideally suited for complex parts requiring fabrication, including deep thermoforming draws and precise molded-in details... |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | Tangent; ASTM D790 |
RheTech Products HP519-00 26% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | Tangent; ASTM D790 |
RheTech Products RCC220-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content Applications: I/P hush panelsSplash shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | 1.3 mm/min; ASTM D790 |
PolyOne Edgetek® X TR2-10TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | Flexural testing speed of 0.5 inches/minute; ASTM D 790 |
NOVA Chemicals Dylark® FG2500 High-Heat Styrenic Copolymer Product Description and Features: Styrenic copolymer with high-heat resistance, high-impact strength and good toughness. Resins used in food grade sheet extrusion and injection molding application.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Global ABS-405 FR High Impact, Flame Retardant ABS Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Conditioned) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Techmer ES HiFill FR® ASA FR-2 WT Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant and Good UV ResistanceAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Spartech 829 Static Conductive Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | tangent; ASTM D790 |
Spartech PE4130 Reinforced High Density Polyethylene Compound Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Star Plastics PC/ABSQX7005 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS 8014 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.14 GPa @Thickness 3.17 mm |
310 ksi @Thickness 0.125 in |
ASTM D790 |
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.14 GPa @Thickness 3.17 mm |
310 ksi @Thickness 0.125 in |
|
TPI Porene® ABS-AN450 Flame Retardant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | 1% Secant; ASTM D790 |
Washington Penn Medium Impact Copolymer 30% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Total PSI 945E Polystyrene Polystyrene 945E is a high impact polystyrene designed for applications requiring extra toughness without sacrificing mechanical properties. Excellent falling dart impact combined with the high glos.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Videolar 825 E High Impact Polystyrene (HIPS) Grade designed specially for extrusion and thermoformingCharacteristics make it especially suitable for industrial packaging deep draw thermoforming and custom multilayer sheet extrusionFeatures: St.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ASA S710 Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Aaron Industries AAROPRENE® CFPP 2030 Calcium Carbonate Filled Polypropylene AAROPRENE® CFPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Proto3000 PC ISO Fused Deposition Modeling Polymer Description: PC-ISO (polycarbonate-ISO), an industrial thermoplastic, which in its raw state, meets the ISO 10993-1 and USP Class VI classi?cation 1. PC-ISO blends are commonly used in food and drug.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790A |
BP Amoco Accpro® 9346 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Long-term heat aging, High stiffness, Nucleated, UL RecognizedComplies with FDA specification, Title 21, CFR 177.1520.Typical applications: .. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | tangent; ASTM D790 |
Spartech EP6120 Filled and Reinforced Copolymer Filled copolymers offer a higher level of impact performance than homopolymer materials, and higher stiffness than unfilled copolymers. Copolymer based materials retain much of their impact strength.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Techmer ES Luriblend® ABS TL10 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel PPA resins, ET-1000 HS offers high fatigue str.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
PlastxWorld CEVIAN® SER20 ABS General purpose and flame retarded ABS with excellent moldability and no plate-out.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Informat.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
PolyOne Edgetek® XT XT-100-CX00 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |