Stir SpA AF 70 R (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Stir SpA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stir SpA AF 70 R (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Flame resistant sheath CEI 20-11 type TM 1Information provided by STIR SpA
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 79
79
ISO 868
Tensile Strength at Break 12.65 MPa
1835 psi
ISO R 527
Elongation at Break 259 %
259 %
ISO R 527
Thermal Properties Metric English Comments
Oxygen Index 29.2 %
29.2 %
ASTM D2863