Material Notes:
Application: Extrusion pipe and sheath CEI 20-11 type TM-2Information provided by STIR SpA
Physical Properties Metric English Comments
Density 1.513 g/cc
0.05466 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ISO 868
Tensile Strength at Break 13.8 MPa
2000 psi
ISO R 527
Elongation at Break 330 %
330 %
ISO R 527