Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Stir SpA SR 90 CZ (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Stir SpA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stir SpA SR 90 CZ (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Extrusion insulation CEI 20-11 type TI-1Information provided by STIR SpA
Physical Properties Metric English Comments
Density 1.525 g/cc
0.05509 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ISO 868
Tensile Strength at Break 15.2 MPa
2200 psi
ISO R 527
Elongation at Break 263 %
263 %
ISO R 527
Users viewing this material also viewed the following: