Struktol MONTAN WAX E Lubricant, Processing Additive

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Struktol
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol MONTAN WAX E Lubricant, Processing Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Montanic ester wax.STRUKTOL® Montan Wax E is an excellent processing additive for PVC. It provides superior plate out properties, wide processing latitude and is ideal for clear applications. Primary applications are for calendered goods, injection, and blow molded products.
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
Additive Loading 0.10 - 0.50 %
0.10 - 0.50 %
Viscosity 15 - 20 cP

@Temperature 120 °C
15 - 20 cP

@Temperature 248 °F
Thermal Properties Metric English Comments
Dropping Point >= 81.0 °C
>= 178 °F
Chemical Properties Metric English Comments
Acid Value <= 20
<= 20
Descriptive Properties Value Comments
Appearance Pale yellow flakes
Penetrometer Value 1
Solidification Point (°C) 78