Struktol TR 065 Blending Aid, Processing Additive

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Struktol
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol TR 065 Blending Aid, Processing Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Blend of medium molecular weight resins designed as a high temperatures process aid and blending agent.Effective in binding filler materials to the polymer system by virtue of its adhesive nature at process temperatures. The components of STRUKTOL® TR 065 should make it compatible with most polymers, polar or non-polar in nature. It should withstand processing temperatures to 370°C. Those systems, which should benefit from both compounding and processing improvements, include high-filled polyesters, nylon, nitriles, PVC and blends or alloys of dissimilar materials. STRUKTOL® TR 065 is an excellent compatibilizer and has proven useful for processing recycle materials.FDA Status: 172.280; 172.615; 175.105; 175.125; 175.300; 175.320; 177.2600; 178.3930
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Additive Loading 0.50 - 1.0 %
0.50 - 1.0 %
Thermal Properties Metric English Comments
Dropping Point 106 - 116 °C
223 - 241 °F
Processing Properties Metric English Comments
Shelf Life >= 24.0 Month
>= 24.0 Month
Descriptive Properties Value Comments
Appearance Light yellow pastilles or powder