Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 106 - 116 °C | 223 - 241 °F | Average value: 109 °C Grade Count:6 |
Overview of materials for Anhydride-Modified Polyethylene This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o.. |
|||
Dropping Point | 106 - 116 °C | 223 - 241 °F | |
Struktol TR 065 Blending Aid, Processing Additive Blend of medium molecular weight resins designed as a high temperatures process aid and blending agent.Effective in binding filler materials to the polymer system by virtue of its adhesive nature at.. |