Struktol TR 131 Slip Agent, Lubricant, Mold Release Agent

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Struktol
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol TR 131 Slip Agent, Lubricant, Mold Release Agent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unsaturated primary amide derived from erucic acid.STRUKTOL® TR 131 is mainly used as a slip agent in polyolefin films, reducing the coefficient of friction. It is the agent of choice at higher extrusion temperatures because of its high heat stability and slower rate of migration to the surface compared with oleamides. The slower rate of migration is also an advantage when films are printed, sealed or laminated shortly after extrusion. Its low odor makes it extremely suitable for food contact applications. STRUKTOL® TR 131 is also used as a release agent in various polymer systems, and as a dispersant in color concentrates and printing inks. In PVC plastisols for screw closures, it reduces the torque and facilitates release. STRUKTOL® TR 131 is also used as a process aid or lubricant in thermoplastic elastomers (TPEs), thermoplastic resins and thermoset rubber systems. The properties it imparts to the surface may assist in subsequent operations such as parts assembly.FDA Status: 175.105; 176.180; 177.1200; 177.1350; 178.3860; 179.45
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
Additive Loading 0.050 - 0.50 %
0.050 - 0.50 %
For plastics (1-3 phr in elastomers)
Thermal Properties Metric English Comments
Melting Point 79.0 - 85.0 °C
174 - 185 °F
Optical Properties Metric English Comments
Gardner Color Number 4.0
4.0
Chemical Properties Metric English Comments
Acid Value <= 3.0
<= 3.0
Processing Properties Metric English Comments
Shelf Life >= 24.0 Month
>= 24.0 Month
Descriptive Properties Value Comments
Amide Content (%) 99
Appearance Off-white pellets or beads
Iodine Value (max) 78