Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 79.0 °C | 174 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 1302 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
(discontinued **) 13 wt% Methacrylic Acid.Nucrel® 1302 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process po.. |
|||
Melting Point | 79.0 °C | 174 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Appeel® LSR 11D569 Modified EVA Lidding Sealing Resin
(discontinued **) Appeel 11D569 is a modified ethylene vinyl acetate copolymer resin designed to be used as a sealing layer for lidding applications. It provides peelable seals to a variety of surfaces including poly.. |
|||
Melting Point | 79.0 - 89.0 °C | 174 - 192 °F | |
Fine Organics FINALUX G1 Lubricant Additive Applications:Lubricant for:rigid PVC pipesconduitsfittingscable compoundsInformation provided by Fine Organics |
|||
Melting Point | 79.0 °C | 174 °F | Eutectic |
Indium Corp. Indalloy® 174 Bi-In-Sn Fusible Alloy Environmentally safe fusible alloy. Contains no lead or cadmium.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 79.0 - 85.0 °C | 174 - 185 °F | |
Struktol TR 131 Slip Agent, Lubricant, Mold Release Agent Unsaturated primary amide derived from erucic acid.STRUKTOL® TR 131 is mainly used as a slip agent in polyolefin films, reducing the coefficient of friction. It is the agent of choice at higher e.. |
|||
Melting Point | 79.0 °C | 174 °F | Peak; Westlake Method |
Westlake Elevate™ EF526 16% Ethylene Vinyl Acetate Copolymer Westlake Elevate™ EF526 resin is a 16% EVA copolymer designed for cast film, extrusion coatings, and thermal laminations.Application/UsesThermal laminationsCast FilmExtrusion CoatingsThis resin gra.. |
|||
Melting Point | 79.0 °C | 174 °F | ASTM D3418 |
Westlake EMAC® SP2252 20.5% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2252 is a 20.5% EMA copolymer containing slip and antiblock. This resin is designed for blown film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal te.. |
|||
Melting Point | 79.0 °C | 174 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3124 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating 9 wt% Vinyl Acetate.Elvax® 3124 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins... |
|||
Melting Point | 79.0 - 81.0 °C | 174 - 178 °F | |
BASF Triphenylphosphine Pellets Formula: C18H15PCAS: 603-35-0Description: Triphenyl phosphine pellets are a colorless solid, and have a faint specific odor. It is insoluble with water. Synonyms: TPP, Triphenylphosphane, Triphenyl.. |
|||
Melting Point | 79.0 - 81.0 °C | 174 - 178 °F | |
BASF Triphenylphosphine Molten Formula: C18H15PCAS: 603-35-0Description: Triphenyl phosphine pellets are a colorless solid, and have a faint specific odor. It is insoluble with water.Synonyms: TPP, Triphenylphosphane, Triphenylp.. |
|||
Melting Point | 79.0 °C | 174 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Appeel® LSR 2044 Modified EVA Lidding Sealing Resin Appeel® 2044 is a blown or cast film resin designed to be a sealing layer for lidding applications. It provides a peelable seal over a broad temperature range to a number of container materials inc.. |