Styrolution Terblend® N NM-21 XP ABS+PA (Conditioned)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend , Nylon
Manufacturer Styrolution
Trade Name Terblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution Terblend® N NM-21 XP ABS+PA (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 36.0 MPa
5220 psi
ISO 527
Elongation at Break 50 %
50 %
Nominal; ISO 527
Elongation at Yield 5.0 %
5.0 %
ISO 527
Tensile Modulus 1.40 GPa
203 ksi
ISO 527
Izod Impact, Notched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
ISO 180
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 179
8.50 J/cm²

@Temperature 23.0 °C
40.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Dielectric Constant 3.8

@Frequency 1.00e+6 Hz
3.8

@Frequency 1.00e+6 Hz
IEC 60250
Descriptive Properties Value Comments
Commercial Status North America
Users viewing this material also viewed the following: